Project Description
There was a need to reduce heat radiation and save energy from a production furnace.
Coating Solution
Preparation was done by cleaning, degreasing and removing concrements (on cold furnace). Afterwards a combined application of HOT PIPE COATING and HOT SURFACE COATING (on hot furnace) was done followed by 2 coats of RUST GRIP.
On the doors, which were the hottest, HOT PIPE COATING of +/-8mm was applied, followed by 4mm of HOT SURFACE COATING to have a smoother finish. On the rest of the furnace 3mm of HOT SURFACE COATING was applied.
Result
Initial surface temperature: 60°C up to 220°C
After Application surface temperature : between 40°C to 65°C
Products we used